MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot E2C™ DX9660 Elastomer Composite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: Cabot’s engineered elastomer composite (E2C™) solutions are designed for superior particle dispersion and enhanced polymer-particle interaction, which results in stronger reinforcement, improved resistance to damage and reduced hysteresis.

Performance Features: E2C dx9660 elastomer composite is designed to have very high level of abrasion resistance and good hysteresis. It features high 300% modulus and dynamic stiffness.

Typical Applications:

  • On road truck tire tread/retreat
  • Non-tire rubber products for high abrasion: Mill liner with high abrasion (Secondary mill); Trommel screen panel; Ultra-high abrasion conveyor belt; High abrasion rubber rack; Other rubber parts with high abrasion

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 84
@Temperature 100 °C
84
@Temperature 212 °F
ML (1+4)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 33.3 MPa4830 psi
Elongation at Break 489 %489 %
300% Modulus 18.2 MPa2640 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT018 / 315753

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.