MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Glyptal 9620 Finishing Varnish
Categories: Other Engineering Material

Material Notes: GLYPTAL 9620 INSULATING VARNISH is a clear air-drying , insulating, and finishing varnish designed for applications where oil, moisture, and acid-resistant coatings are desired. This fast-drying, synthetic-resin-type varnish is often used as a final coat over other varnishes, giving a hard, glossy protective coating. GLYPTAL 9620 Varnish has excellent heat resistance and will operate as a finish coat at temperatures up to 130 ºC on an apparatus that is not flexed. Although primarily an air-drying varnish, the oil, moisture, acid, and salt water resistance are greatly improved by baking. GLYPTAL 9620 has excellent adhesion to most materials. It has excellent dip tank stability where the proper thinners are used.

APPLICATIONS

GLYPTAL 9620 is suggested as a general-purpose insulating and finishing varnish for form and random-wound coils, stators, armatures, and most other types of electrical apparatuses. It is excellent for giving and oil-resistant finish coating over inexpensive asphalt varnishes

GLYPTAL 9620 has also found many uses as a fast-drying, general purpose adhesive, protective coating, and insulating varnish. It is especially suggested for treatment of small windings where air-drying or short-baking cycles are required.

GLYPTAL 9620 is compatible with systems using varnished cloth, cotton, rayon, Dacron, polyester fiber, nylon, glass tapes, laminates, slot liners and slot wedges, mica products, Irrathene, irradiated polyethylene, mylar film, oleoresinous and Formvar wire enamels, vinyl and acetate products, metals, braided wires and cables, and most other materials found in electrical equipment.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Solids Content 38 - 42 %Weight
Viscosity 300 - 500 cPMacMichael
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 2500 V/milDry; ASTM D115-55
 600 V/mil
@Time 86400 sec
In Water; ASTM D115-55
 
Thermal PropertiesOriginal ValueComments
Flash Point 66.0 °FPensky-Martens
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 0.500 hourAir Dry, 1 mil dry film
 
Descriptive Properties
Chemical ResistanceExcellentOil (Transil)
 FairAlkali
 GoodWater
 GoodSalt Water
 GoodAcid
Solvent SystemXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane
Pearl Engineering PEPLPET B-101C PET Sheet Grade
Nylene® 615 Nylon 6, Film Grade
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane

PGLYPT915 / 209754

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.