MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® EX9350 BK E70293 Nylon 612, Impact Modified, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Impact Modified

Material Notes: VESTAMID® EX9350 BK E70293 is a PA 612 elastomer extrusion compound developed for the manufacturing of tubing systems, e.g. vacuum brake booster lines. The compound is in particular suitable for applications, that require a continuous high flexibility even if subjected to high temperature load. In contrast to conventionally plasticized materials (plasticizerloss) tubes made from VESTAMID® EX9350 BK E70293 do not stiffen under elevated temperatures. In comparison with PA 11 and PA 12 compounds the increased melting point allows for increased peak temperatures in use. The compound is especially suitable for the extrusion of tubing systems that are exposed to increased burst pressures and service temperatures. The process temperatures should be within a range of 210 to 240 °C. VESTAMID® EX9350 BK E70293 is supplied as cylindrical pellets in moisture-proof packaging, ready for use. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Industry and Engineering
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: High impact strength, Light-stabilized, High heat resistant
Color: Black
Additives: Impact resistant, Heat stabilizer

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Water Absorption 1.10 %Sim to ISO 62
Moisture Absorption 3.50 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.0110 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0100 cm/cmISO 294-4, 2577
Melt Flow 56.0 g/10 min
@Load 2.16 kg,
Temperature 280 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67.0
@Time 3.00 sec
ISO 7619-1
Tensile Strength at Break 41.0 MPaISO 527
Tensile Strength 30.0 MPaISO 527
Tensile Stress 46.5 MPaTPE; ISO 527
 22.5 MPa
@Strain 5.00 %
ISO 527
 27.6 MPa
@Strain 10.0 %
ISO 527
 28.6 MPa
@Strain 50.0 %
ISO 527
 29.0 MPa
@Strain 50.0 %
ISO 527
 29.4 MPa
@Strain 100 %
ISO 527
 30.0 MPa
@Strain 20.0 %
ISO 527
 50.2 MPa
@Strain 300 %
ISO 527
Tensile Strength, Yield 30.0 MPaISO 527
Elongation at Break 276 %TPE; ISO 527
 330 %Nominal; ISO 527
Elongation at Yield 30.0 %ISO 527
Tensile Modulus 630 MPaISO 527
Flexural Strength 19.0 MPaat conv. Deflection; ISO 178
 28.0 MPaISO 178
Flexural Modulus 615 MPaISO 178
Flexural Strain at Break 9.00 %at flexural strength; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature 0.000 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -40.0 °C
Type of failure: C; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 30.0 kJ/m²
@Temperature 23.0 °C
Type of failure: P; ISO 179/1eA
Impact <= NBwith pendulum, pipe, -40°C; Tube dimension: OD x WT 12x1.25 mm; DIN 73378
 0.000
@Temperature -40.0 °C
Cold impact resistance, breaks of 10, 880g; Sim. to VW Audi PV 3905
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.60e+8 ohm-cmIEC 62631-3-1
Surface Resistance >= 7.00e+11 ohmIEC 62631-3-2
Dielectric Constant 3.40
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 8.30
@Frequency 100 Hz
IEC 62631-2-1
 9.20
@Frequency 50.0 Hz
IEC 62631-2-1
Dielectric Strength 35.0 kV/mmAC, S20/S20, t.; IEC 60243-1
Dissipation Factor 0.0616
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.294
@Frequency 100 Hz
IEC 62631-2-1
 0.354
@Frequency 50.0 Hz
IEC 62631-2-1
Comparative Tracking Index 575 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 122 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 198 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Vicat Softening Point 130 °C
@Load 5.10 kg
50 K/h; ISO 306
 186 °C
@Load 1.02 kg
50 K/h; ISO 306
Glass Transition Temp, Tg -4.00 °CISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °C
Mold Temperature 35.0 °C
 
Descriptive Properties
ColorBlack
Flexural stress at breakNMPa, ISO 178
 N%, ISO 178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7904 / 325036

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.