MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adstif HA 840R Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability.

Adstif HA840R is a nucleated homopolymer which features very high crystallinity, outstanding rigidity and high gloss. Adstif HA840R is selected for the production of stiff injection molded articles where high rigidity is needed. Typical applications of Adstif HA840R include food packaging containers, house wares, small appliances and technical parts.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.0 MPa5950 psiISO 527-1,-2
Elongation at Break 12 %12 %ISO 527-1,-2
Elongation at Yield 6.0 %6.0 %ISO 527-1,-2
Tensile Modulus 2.30 GPa334 ksiISO 527-1,-2
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 158 °C316 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Gloss 95 %95 %@60°; ASTM D 2457
 
Descriptive Properties
Processing MethodInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Addiplast Addilene H 530 N30 Polypropylene Homopolymer
Borealis Borcom™ WG140AI Polypropylene
NCMT NanoPAC™ G1000 High Performance Polypropylene Nanocomposite
Overview of materials for High Density Polyethylene (HDPE), Wood Filled
Overview of materials for Polypropylene, Molded

PEQT7018 / 218657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.