MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC LNP™ THERMOCOMP™ XF006S Nylon (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: LNP THERMOCOMP XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Density 1.36 g/cc0.0491 lb/in³ASTM D792
Moisture Absorption 0.220 %0.220 %50% RH, 24 hrs; ASTM D570
 0.280 %0.280 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24HRS; ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in24 HRS; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 138 MPa20000 psi5 mm/min; ASTM D638
 141 MPa20500 psi5 mm/min; ISO 527
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527
 2.6 %2.6 %5 mm/min; ASTM D638
Tensile Modulus 9.02 GPa1310 ksi1 mm/min; ISO 527
 9.65 GPa1400 ksi50 mm/min; ASTM D638
Flexural Strength 208 MPa30200 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 214 MPa31000 psiISO 178
Flexural Yield Strength 209 MPa30300 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8.91 GPa1290 ksi2 mm/min; ISO 178
 9.06 GPa1310 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.560 J/cm1.05 ft-lb/inASTM D256
Izod Impact, Unnotched 6.32 J/cm11.8 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 38.0 kJ/m²18.1 ft-lb/in²80*10*4; ISO 180/1U
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
Instrumented Impact Total Energy 11.0 J8.11 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 44.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
24.4 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 35.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 144 °C291 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 142 °C
@Thickness 3.20 mm
288 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 138 °C
@Thickness 3.20 mm
280 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 1 260 - 270 °C500 - 518 °F
Zone 2 270 - 290 °C518 - 554 °FInjection Molding
Zone 3 290 - 300 °C554 - 572 °F
Melt Temperature 260 - 300 °C500 - 572 °FInjection Molding
Mold Temperature 50.0 - 100 °C122 - 212 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 6.00 - 12.0 hour6.00 - 12.0 hourInjection Molding
Moisture Content 0.10 %0.10 %Injection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH91728 / 252852

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.