MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
TPC Group DIISOBUTYLENE
Categories: Other Engineering Material

Material Notes: Characteristics: TPC Group manufactures a high purity diisobutylene (DIB) product based on the polymerization of isobutylene.

Applications: DIB is used as a building block raw material for lubricants, dispersants, anti-wear additives, surfactants, silicones, industrial fluids, oxidation inhibitors, and rubber processing chemicals. Preferred diisobutylene-based products include octylphenols, isononyl alcohol, octylsilanes, isononanoyl derivatives, and octylthiols. DIB can also be hydrogenated to saturate the double bond to form isooctane, which is a key component of C8 alkylate.

General: TPC Group’s DIB is a high purity isoolefin that is primarily a mixture of two primary isomers: 2,4,4-trimethylpentene-1 and 2,4,4-trimethylpentene-2.

Packaging: DIB is sold in railcar quantities, however, trucks and barge quantities are also available.

Information provided by TPC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AppearanceClear and Free of Entrained Matter
Assay>98.5%Diisobutylene Assay (Dimer 1 + Dimer 2), Min, DIB-001
 0.99Diisobutylene Assay (Dimer 1 + Dimer 2), Typical, DIB-001
Color<1Pt-Co, Typical, ASTM D-1209
 <25Pt-Co, Max, ASTM D-1209
Content<1 ppmSulfur, Typical, HNO-632
 <10 ppmSulfur, Max, HNO-632
 50-100 ppmInhibitor (BHT), DIB-002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTPCG001 / 320503

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.