MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Total PPH 3576XHD Polypropylene Homopolymer, Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Low Residuals TOTAL Polypropylene 3576XHD utilizes the new ATOFINA proprietary process technology to provide extremely low residuals for improved color stability and clarity.

Antiblock. 3576XHD is formulated with a special antiblock additive.

FDA. 3576XHD complies with all applicable FDA regulations for food contact applications.

Recommended Applications. TOTAL Polypropylene 3576XHD is recommended for use in non-oriented cast film processes for manufacture of packaging films.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Water Vapor Transmission 1.20 g/100 in²/day
@Temperature 37.8 °C
90% RH; ASTM F1249-90
Melt Flow 9.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8000 psiASTM D882
Elongation at Break 500 %ASTM D882
Secant Modulus 115 ksiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %ASTM D1003
Gloss 75 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 450 - 525 °FCast Film Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3576 H Polypropylene Homopolymer, Cast Film
Total PPH 5069 Polypropylene Homopolymer, Fiber
Ineos H08U-00 Polypropylene Homopolymer, Fiber Grade
Borealis HD234CF Polypropylene
BASF Novolen® 3325 MC Polypropylene

PTOTAL813 / 130538

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.