MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³
Linear Mold Shrinkage, Flow 0.0135 - 0.0165 cm/cm0.0135 - 0.0165 in/in
Linear Mold Shrinkage, Transverse 0.0135 - 0.0165 cm/cm0.0135 - 0.0165 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  8.00 MPa
@Temperature 90.0 °C
1160 psi
@Temperature 194 °F
 10.0 MPa
@Temperature 60.0 °C
1450 psi
@Temperature 140 °F
 12.0 MPa
@Temperature 23.0 °C
1740 psi
@Temperature 73.4 °F
Elongation at Break  >= 100 %
@Temperature 23.0 °C
>= 100 %
@Temperature 73.4 °F
 >= 100 %
@Temperature 60.0 °C
>= 100 %
@Temperature 140 °F
 >= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
Elongation at Yield  5.7 %
@Temperature 23.0 °C
5.7 %
@Temperature 73.4 °F
 7.0 %
@Temperature 60.0 °C
7.0 %
@Temperature 140 °F
 7.5 %
@Temperature 90.0 °C
7.5 %
@Temperature 194 °F
Tensile Modulus  0.350 GPa
@Temperature 90.0 °C
50.8 ksi
@Temperature 194 °F
 0.550 GPa
@Temperature 60.0 °C
79.8 ksi
@Temperature 140 °F
 1.20 GPa
@Temperature 23.0 °C
174 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 9.00 J/cm²42.8 ft-lb/in²
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F
Vicat Softening Point 75.0 °C
@Load 5.00 kg
167 °F
@Load 11.0 lb
Flammability, UL94  V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Oxygen Index 26 %26 %
Glow Wire Test  850 °C
@Thickness 1.00 mm
1560 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature  750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
 775 °C
@Thickness 2.00 mm
1430 °F
@Thickness 0.0787 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 200 °C356 - 392 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 70.0 - 90.0 °C
@Time 10800 sec
158 - 194 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLATH9775 / 177471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.