Pro-fax RP382U clarified, easy molding, very high flow polypropylene random copolymer is available in pellet form. This resin is typically used in injection molding applications requiring excellent processability and good see-through and contact clarity. Applications: Clear Containers, Multi Media PackagingInformation provided by LyondellBasell. |