MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECAGLIDE black Nylon 6, Lubricant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes:
  • excellent slip-stick properties
  • excellent wear resistance
  • good machinability
  • resistant to many oils, greases and fuels
  • high toughness
  • high mechanical load capacity
Target Industries:
  • conveyor technology
  • construction industry
  • heavy duty industry
  • packaging and paper machinery

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Moisture Absorption 2.50 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9200 psiafter equilibrium @ 50% rel humidity; ASTM D 638
 12000 psiASTM D 638
Elongation at Break 10 %ASTM D 638
 17 %after equilibrium @ 50% rel humidity; ASTM D 638
Modulus of Elasticity 472 ksiafter equilibrium @ 50% rel humidity; ASTM D 638
 520 ksiASTM D 638
Flexural Modulus 435000 psiASTM D 790
Izod Impact, Unnotched 3.40 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.12
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM D 696
Melting Point 420 °F
Maximum Service Temperature, Air 212 °FLong Term
 300 °FShort Term
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8161 / 319089

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.