Product Description: FRblend® PP-1501 is a high flow, mineral filled, flame retardant polypropylene compound comply with UL94 V-2 flammability rating at 1.6mm thickness. It can be colored to meet stringent aesthetic requirements Features: Uses:- Electrical/Electronic components
- Automotive applications
Forms:Processing Method:Information provided by Colour Image Plastic Compound Sdn Bhd |