MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical AF-325 ABS Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: High flow, 5VA, Applications include televisions, VTR monitors, computer and other electrical, electric parts requiring flame retardant properties

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 54 g/10 min
@Load 10.0 kg,
Temperature 220 °C
54 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 41.0 MPa5950 psi50 mm/min; ASTM D638
Elongation at Break 20 %20 %50 mm/min; ASTM D638
Modulus of Elasticity 2.14 GPa310 ksi50 mm/min; ASTM D638
Flexural Yield Strength 67.0 MPa9720 psi50 mm/min; ASTM D790
Flexural Modulus 2.40 GPa348 ksi15 mm/min; ASTM D790
Izod Impact, Notched  2.30 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
4.31 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 2.60 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
4.87 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance <= 60 sec<= 60 secUL Rating PLC 7 (<60 sec)
Comparative Tracking Index 400 - 600 V400 - 600 VUL Rating PLC 1 (400-600 volts)
Hot Wire Ignition, HWI 60 - 120 sec60 - 120 secUL Rating PLC 1 (60-120 sec)
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsUL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL Rating PLC 2 (25.4-80 mm/min)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 6.35 mm
167 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 87.0 °C189 °F1000 g; ASTM D1525
Flammability, UL94  5VA
@Thickness 1.59 mm
5VA
@Thickness 0.0625 in
FVO mm/min per IEC 707; UL94
 5VA
@Thickness 1.59 mm
5VA
@Thickness 0.0625 in
FVO mm/min per IEC 707; UL94
 5VA
@Thickness 3.17 mm
5VA
@Thickness 0.125 in
UL94
 5VA
@Thickness 3.17 mm
5VA
@Thickness 0.125 in
UL94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® FR 7087 Polycarbonate
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade
Avient Maxxam™ FR PP 402 Polypropylene
Avient Maxxam™ FR PP 401 CS Polypropylene

PLAZ52 / 50310

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.