MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Westlake EF 442 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Applications
  • Compounding
Properties
  • Excellent Toughness
  • High Flow
  • High Gloss
  • Low Warpage Tendency and Excellent Cold Crack

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520, paragraph C, section 2.1, for use in articles that contact food. Kosher approved

Processing: Extrusion melt temperatures of 330° to 360°F are recommended for Westlake Polymers EF 442

Information provided by Westlake Chemical Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 26 g/10 min26 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 8.27 MPa1200 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Tensile Modulus 0.141 GPa20.5 ksiASTM D1709
Flexural Stiffness 120 MPa17400 psiASTM D747
Torsional Stiffness 159 MPa23100 psiASTM D1043
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 85.0 °C185 °FASTM D1525
Brittleness Temperature -56.0 °C-68.8 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 166 - 182 °C330 - 360 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
NOVA Chemicals Novapol® LM-2522-A LDPE Injection Molding Resin
SCG Chemicals EL-Lene™ LD1630J Low Density Polyethylene Injection Molding
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Chevron Phillips Marlex® 1412 Injection Molding Resin

PWESG032 / 72678

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.