MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Vistalon™ 722 Ethylene Propylene Copolymer Rubber - Wire and Cable
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Vistalon 722 rubber is copolymer rubber designed for medium and low voltage wire and cable applications and is produced using ExxonMobil Chemical's EXXPOL™ Technology for precise control of molecular composition and architecture. This product is sold in pellet form.

Key Features: Designed for good electrical properties, easy processing of cables and cable compounds, enhanced cable flexibility and low temperature performance.

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 17
@Temperature 125 °C
17
@Temperature 257 °F
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Estimate from melt flow rate data; ExxonMobil Method
 
Descriptive Properties
Ethylene Content72.0 wt%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Vistalon™ 404 Ethylene Propylene Copolymer Rubber
Geon® Performance Solutions 82520 Fiberloc PVC; 20% Glass Fiber Reinforced
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid
ExxonMobil Vistalon™ 878P Ethylene Propylene Copolymer Rubber
ExxonMobil Vistalon™ 706 Ethylene Propylene Copolymer Rubber

PEXA932 / 125975

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.