MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemical Concepts Ultralok 421GB Structural Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: The Chem-set™ Ultralok 420GB, 421GB and 422GB are high performance two part structural adhesives engineered to bond a wide range of plastics, metals, and composite materials. These products feature superior bond strength and extreme durability, with excellent impact and weathering properties. The Ultralok 400 series offer improved performance, ease of use and reliability over competing adhesives. The Ultralok series adhesives are available in several versions with faster or slower curing speeds to optimize the application process to your specific needs and ambient temperature. The integrated glass beads act as spacers to maintain consistent bondline thickness resulting in stronger joints and preventing failure due to over-clamping.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 - 1.05 g/cc0.930 - 1.05 g/ccadhesive
Density 0.923 - 1.05 g/cc0.0333 - 0.0381 lb/in³Adhesive. Relative
Volatile Organic Compounds (VOC) Content <= 50 g/l<= 50 g/ladhesive
pH 4.0 - 6.04.0 - 6.0adhesive
 4.0 - 6.04.0 - 6.0activator
Vapor Pressure  <= 0.000667 bar
@Temperature 20.0 °C
<= 0.500 torr
@Temperature 68.0 °F
Activator
 0.0373 bar
@Temperature 20.0 °C
28.0 torr
@Temperature 68.0 °F
Adhesive
 
Thermal PropertiesMetricEnglishComments
Melting Point -47.8 °C-54.0 °Fadhesive
Boiling Point 100 °C212 °Fadhesive
 >= 288 °C>= 550 °Factivator
Flash Point 10.0 °C50.0 °Fadhesive. Tag Closed Cup
 
Descriptive Properties
AppearanceLiquid (activator)
Auto Ignition Temperature790°F. Adhesive
ColorVarious colored paste (adhesive)
Evaporation Point<1 (activator)
 3( adhesive)
Flammability TestClass 1B (activator)
 Class 1B (adhesive)
Odormild sweet (activator)
 mild sweet (adhesive)
Vapor Density3.5 (air=1) adhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI991 / 232238

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.