Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. Advantages & Application Notes: - Built in color change from clear to amber when cured properly. The color change can be used for in-line inspection of epoxy joints and adhesive fillet.
- Unfilled epoxy resin allows for % transmission in the VIS and NIR.
- Low viscosity allows for wicking and capillary action.
- Suggested Applications:
- Semiconductor: capillary flow underfill for Flip Chip mounted die
- Fiber Optic: polarizing maintaining fibers (PMF) found in gyroscope coils; fiber termination into ferrule.
- Medical: impregnation into fiber optic light guides and endoscopes; resists autoclave, ETO, or gamma sterilization.
Information Provided by Epoxy Technology |