Pro-fax SG722 fully formulated high impact polypropylene copolymer is available in pellet form. This resin is typically used in injection molding applications and offers very good cold temperature impact resistance. Applications: Containers, House wares, Sports, Leisure & ToysInformation provided by LyondellBasell. |