MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
VICTREX AM™ 450 FIL PEEK 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: High performance thermoplastic material, PolyEtherEtherKetone (PEEK), semi crystalline, filament for Additive Manufacture by filament fusion and other melt extrusion 3D printing processes.

Uses: Additive manufacturing processing. Filament Fusion printed parts. For use in high temperature applications and chemically aggressive environments. Low outgassing, suitable for sterilization. Not suitable for medical implant applications. Product supplied vacuum packed with desiccant and dry when produced. Drying before use is recommended. This product is based on VICTREX™ PEEK 450G.

Property data from INTAMSYS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccCrystalline; ISO 1183
Water Absorption at Saturation 0.45 %
@Temperature 23.0 °C
Immersion; ISO 62-1
 0.55 %
@Temperature 100 °C
Immersion; ISO 62-1
Viscosity 350000 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 84.5ISO 11443
Tensile Strength, Yield 0.0200 - 0.0800 GPaVertical Orientation Filament Extrusion; ISO 527
 0.0600 - 0.0800 GPaHorizontal Orientation Filament Extrusion; ISO 527
 0.0980 GPaInjection Molded; ISO 527
Elongation at Break 1.0 - 10 %Vertical Orientation Filament Extrusion; ISO 527
 45 %Injection Molded; ISO 527
 2.0 - 95 %Horizontal Orientation Filament Extrusion; ISO 527
Tensile Modulus 2.00 - 4.00 GPaVertical Orientation Filament Extrusion; ISO 527
 3.00 - 4.00 GPaHorizontal Orientation Filament Extrusion; ISO 527
 4.00 GPaInjection Molded; ISO 527
Flexural Strength 12.5 ksi
@Strain 3.5 %,
Temperature 275 °C
Injection Molded; ISO 178
 19.0 ksi
@Strain 3.5 %,
Temperature 175 °C
Injection Molded; ISO 178
 85.0 ksi
@Strain 3.5 %,
Temperature 125 °C
Injection Molded; ISO 178
 125 ksi
@Strain 3.5 %,
Temperature 23.0 °C
Injection Molded; ISO 178
Flexural Modulus 3.80 GPaInjection Molded; ISO 178
Compressive Strength 70.0 MPa
@Temperature 120 °C
Injection Molded; ISO 604
 125 MPa
@Temperature 23.0 °C
Injection Molded; ISO 604
Izod Impact, Notched (ISO) 7.00 kJ/m²Injection Molded; ISO 180/A
Izod Impact, Unnotched (ISO) NBInjection Molded; ISO 180/U
Charpy Impact Unnotched NBInjection Molded; ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²Injection Molded; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 23.0 kV/mmIEC 60243-1
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.290 W/m-K
@Temperature 23.0 °C
Average; ISO 22007-4
 0.320 W/m-K
@Temperature 23.0 °C
Along Flow; ISO 22007-4
Melting Point 343 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 152 °CISO 75-f
Glass Transition Temp, Tg 143 °CDSC Onset; ISO 11357
 150 °CDSC Midpoint; ISO 11357
UL RTI, Electrical 260 °CUL746B
UL RTI, Mechanical with Impact 180 °CUL746B
UL RTI, Mechanical without Impact 240 °CUL746B
Glow Wire Test 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= 150 °CChamber/Build-Space Example
 >= 150 °CBed Example
 340 - 450 °CExtrusion Example
Drying Temperature 120 °C
@Time 18000 sec
Example
Moisture Content <= 0.020 %Example
 
Descriptive Properties
Colornatural/beige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVICTB880e / 305341

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.