MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolon® 622R PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Homopolymer General Purpose Grade Resin

F622R is a medium-low molecular weight PVC homopolymer of interest in both rigid and flexible applications and has established a deserved reputation for low gels, and exceptional early color heat stability. These properties, along with outstanding lot to lot uniformity, have made F622R an industry wide standard for both rigid and flexible formulations.

Applications: Rigid and Flexible Calendering, Rigid Foam, Profile and Bottles

ASTM Classification: GP3-16000, ASTM D1755

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.560 g/cc0.0202 lb/in³ASTM D1895
Volatiles 0.20 %0.20 %ASTM D6980
Particle Mesh Size 40 Mesh40 Mesh99.9% thru; Malvern
 200 Mesh200 Mesh6% thru; Malvern
Viscosity 0.81 cP0.81 cPInherent; ASTM D5225
Relative Viscosity 2.01 cP2.01 cP
 
Descriptive Properties
Composition<1.0 ppmResidual VCM, GC Head Space Method
 20Contamination Count, OCS per 100g
K-Value62Fikentscher's Constant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary PVC 7731 Polyvinyl Chloride Thermoplastic
AlphaGary PVC 7732 Polyvinyl Chloride Thermoplastic
AlphaGary PVC GEX 03-033 F Natural Polyvinyl Chloride Thermoplastic
Axiall 1025-115A Flexible PVC
Axiall 1601 Clear 7002 Flexible PVC

PFPCPQ085 / 150317

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.