MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Raschig Group MELOPAS® 2010 MF Melamine
Categories: Polymer; Thermoset; Melamine

Material Notes: Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection and compression molding

Primary application: Mountings for household appliances, car ash-trays

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 - 1.70 g/cc1.50 - 1.70 g/ccISO 1183
Apparent Bulk Density 0.550 - 0.750 g/cc0.0199 - 0.0271 lb/in³ISO 60
Water Absorption <= 2.0 %
@Temperature 23.0 °C,
Time 86400 sec
<= 2.0 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm0.0050 - 0.010 in/inCompression; ISO 2577
 0.0080 - 0.013 cm/cm0.0080 - 0.013 in/inInjection; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 - 65.0 MPa5800 - 9430 psiCompression; ISO 527
 50.0 - 90.0 MPa7250 - 13100 psiInjection; ISO 527
Modulus of Elasticity 5.00 - 8.00 GPa725 - 1160 ksiInjection and Compression; ISO 527
Flexural Strength 90.0 - 120 MPa13100 - 17400 psiCompression; ISO 178
 100 - 130 MPa14500 - 18900 psiInjection; ISO 178
Flexural Modulus 8.00 - 9.00 GPa1160 - 1310 ksiInjection and Compression; ISO 178
Compressive Strength 200 - 250 MPa29000 - 36300 psiISO 604
Charpy Impact Unnotched 0.600 - 0.900 J/cm²2.86 - 4.28 ft-lb/in²Compression; ISO 179/1eU
 0.800 - 1.40 J/cm²3.81 - 6.66 ft-lb/in²Injection; ISO 179/1eU
Charpy Impact, Notched 0.140 - 0.200 J/cm²0.666 - 0.952 ft-lb/in²Compression; ISO 179/1eA
 0.150 - 0.200 J/cm²0.714 - 0.952 ft-lb/in²Injection; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm1.00e+11 - 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+10 - 1.00e+11 ohm1.00e+10 - 1.00e+11 ohmIEC 60093
Dielectric Constant  7.0 - 9.0
@Frequency 1e+6 Hz
7.0 - 9.0
@Frequency 1e+6 Hz
IEC 60250
 11 - 16
@Frequency 100 Hz
11 - 16
@Frequency 100 Hz
IEC 60250
Dielectric Strength 15.0 - 20.0 kV/mm381 - 508 kV/inIEC 60243-1
Dissipation Factor  0.030 - 0.050
@Frequency 1e+6 Hz
0.030 - 0.050
@Frequency 1e+6 Hz
IEC 60250
 0.30 - 0.50
@Frequency 100 Hz
0.30 - 0.50
@Frequency 100 Hz
IEC 60250
Arc Resistance 120 - 180 sec120 - 180 secASTM D495
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 35.0 µm/m-°C
@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F
@Temperature 122 - 212 °F
ISO 11359-2
Thermal Conductivity 0.400 - 0.500 W/m-K2.78 - 3.47 BTU-in/hr-ft²-°FASTM E1461
Maximum Service Temperature, Air  135 °C
@Time 7.20e+7 sec
275 °F
@Time 20000 hour
IEC 60216/T1
 160 °C
@Time <=180000 sec
320 °F
@Time <=50.0 hour
IEC 60216/T1
Deflection Temperature at 1.8 MPa (264 psi) 155 - 180 °C311 - 356 °FISO 75-A
Deflection Temperature at 8.0 MPa 110 - 130 °C230 - 266 °FISO 75-C
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 1.0 - 1.5 %
@Temperature 110 °C,
Time 605000 sec
1.0 - 1.5 %
@Temperature 230 °F,
Time 168 hour
Post shrinkage; ISO 2577
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
6.00 Month
@Temperature 59.0 - 77.0 °F
 
Descriptive Properties
Glow wire flammability test960/1IEC 60695 2-12
Glow wire ignitability test900/1IEC 60695 2-13
Water Absorption<115 mg24 hr, 23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Conditioned, 30% Glass Filled
Avient Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
Bayshore Vinyl Compounds BRC R409002 Molding Compound

PRASCI02 / 179139

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.