Excels in Air Impermeability, Weather Resistance, Ozone Resistance, Heat Resistance, and Aging Resistance. The heat aging resistance is improved for chlorobutyl and bromobutyl in comparison with regular butyl rubber. Characteristics: Excels in heat & Chemical Resistance. Application: Automotive parts, bladder, heat resistance hose, lining ENEOS has acquired the elastomer product lines from JSR Corporation. |