MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.

Applications: House-wares, lids, closures and toys.

Advantages: Excellent stress crack resistance, toughness and gloss, superior molding properties, low odor.

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.918 g/ccASTM D1505
ESCR 100% Igepal® 150 hour
@Thickness 3.80 mm,
Temperature 23.0 °C
slit; ASTM D1693
Base Resin Melt Index 25 g/10 minI2; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8.83 MPaASTM D638
Tensile Strength, Yield 11.8 MPaASTM D638
Elongation at Break >= 200 %ASTM D638
1% Secant Modulus 42670 psiASTM D638
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 85.0 °Cresin; ASTM D1525
Brittleness Temperature <= -70.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 220 °C
Mold Temperature 10.0 - 40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Chemical Titan TITANEX® LI5011 Linear low density polyethylene resin
Multibase Multi-Pro® 2516 CU Polypropylene
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin

PTITAN46 / 70412

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.