MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping behavior.

Triax® is now a INEOS Styrolution trade name; this grade is discontinued. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccdry as molded
Linear Mold Shrinkage 0.0045 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 69ASTM D785
Tensile Strength, Ultimate 32.0 MPaASTM D638
Tensile Strength, Yield 27.0 MPa
Elongation at Break 90 %ASTM D638
Elongation at Yield 11 %
Tensile Modulus 0.900 GPa
Flexural Yield Strength 61.0 MPaat 5% strain; ASTM D790
Flexural Modulus 1.70 GPaASTM D790
Izod Impact, Notched 9.00 J/cm
@Thickness 3.20 mm
ASTM D256
 1.00 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
ASTM D256
Charpy Impact Unnotched NB
 2.30 J/cm²
@Temperature -30.0 °C
Charpy Impact, Notched 7.00 J/cm²
Impact Test 61.0 J
@Thickness 3.20 mm
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 3.3 m/s; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 9.00e+12 ohm-cmASTM D257
Surface Resistance 3.20e+13 ohmASTM D257
Dielectric Constant 3.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 1.60 mm
Short time under oil; ASTM D149
Dissipation Factor 0.039
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
Vicat Softening Point 94.0 °C
UL RTI, Electrical 60.0 °C
UL RTI, Mechanical with Impact 60.0 °C
UL RTI, Mechanical without Impact 60.0 °C
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned)
INEOS Styrolution Terblend® N NMX04 ABS/PA6 (Dry)
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)

PBA593 / 27031

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.