MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.

Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquids.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes...

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 135 MPaISO 527 Type 1A
Tensile Stress at Strain 25.0 MPa
@Strain 1 %,
Temperature 150 °C
 30.0 MPa
@Strain 1 %,
Temperature 120 °C
 40.0 MPa
@Strain 1 %,
Temperature 80.0 °C
 40.0 MPa
@Strain 2 %,
Temperature 150 °C
 50.0 MPa
@Strain 2 %,
Temperature 120 °C
 50.0 MPa
@Strain 3 %,
Temperature 150 °C
 55.0 MPa
@Strain 1 %,
Temperature 23.0 °C
 55.0 MPa
@Strain 4 %,
Temperature 150 °C
 60.0 MPa
@Strain 3 %,
Temperature 120 °C
 65.0 MPa
@Strain 4 %,
Temperature 120 °C
 65.0 MPa
@Strain 8.0 %,
Temperature 150 °C
 70.0 MPa
@Strain 2 %,
Temperature 80.0 °C
 70.0 MPa
@Strain 8.0 %,
Temperature 120 °C
 75.0 MPa
@Strain 1 %,
Temperature 0.000 °C
 75.0 MPa
@Strain 3 %,
Temperature 80.0 °C
 80.0 MPa
@Strain 4 %,
Temperature 80.0 °C
 80.0 MPa
@Strain 8.0 %,
Temperature 80.0 °C
 95.0 MPa
@Strain 2 %,
Temperature 23.0 °C
 100 MPa
@Strain 1 %,
Temperature -40.0 °C
 110 MPa
@Strain 3 %,
Temperature 23.0 °C
 115 MPa
@Strain 4 %,
Temperature 23.0 °C
 135 MPa
@Strain 2 %,
Temperature 0.000 °C
 150 MPa
@Strain 3 %,
Temperature 0.000 °C
 155 MPa
@Strain 4 %,
Temperature 0.000 °C
 175 MPa
@Strain 2 %,
Temperature -40.0 °C
Elongation at Break 7.0 %ISO 527 Type 1A
Tensile Modulus 7500 MPaISO 527 Type 1A
Flexural Strength 185 MPaISO 178
Flexural Modulus 6400 MPaISO 178
Izod Impact, Unnotched (ISO) 18.0 kJ/m²ISO 180/1eU
Charpy Impact Unnotched 88.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 4.0IEC 60250
Dielectric Strength 29.0 kV/mmIEC 60243
Dissipation Factor 0.11IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Envalior Durethan® AKV 30 HR H2.0 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Conditioned
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, Conditioned
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, Conditioned
BASF Polystyrol® 473 D Impact Grade Polystyrene (Europe)

PRHOD638 / 137869

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.