MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Denka SR-Q ABS Polymer, Chemical Resistant Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Excellent chemical resistance, good flow.

This product uses the fourth component with a micro dispersed structure that helps create a uniform morphology while maintaining the basic properties of ABS resins. It has good chemical resistance to environmental stress cracking, and can be dissolved in chemical solvents for ABS. Therefore, this product cannot be used in containers for organic solvents or other products constantly contacting solvents. Uses: Refrigerator parts (inner boxes and door handles) and toiletry products.

Information provided by Denka Company Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D-792
 1.06 g/cc0.0383 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 2.00 mm
0.0040 - 0.0060 in/in
@Thickness 0.0787 in
DENKA Method
Melt Flow 17 g/10 min
@Load 9.99 kg,
Temperature 220 °C
17 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ISO 2039-2
 110110ASTM D-785
Tensile Strength at Break 36.0 MPa5220 psi50 mm/min; ISO 527-1,-2
 45.0 MPa6530 psi5 mm/min; ASTM D-638
Tensile Strength, Yield 48.0 MPa6960 psi50 mm/min; ISO 527-1,-2
Tensile Modulus 2.45 GPa355 ksi1 mm/min; ISO 527-1, -2
Flexural Strength 72.0 MPa10400 psi15 mm/min; ASTM D-790
 74.0 MPa10700 psi2 mm/min; ISO 178
Flexural Modulus 2.35 GPa341 ksi2 mm/min; ISO 178
 2.40 GPa348 ksi15 mm/min; ASTM D-790
Izod Impact, Notched 1.64 J/cm3.07 ft-lb/inASTM D-256
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FFlatwise; ISO 75-1, -2
 88.0 °C190 °FEdgewise; ASTM D-648
Vicat Softening Point  98.0 °C
@Load 5.10 kg
208 °F
@Load 11.2 lb
ASTM D-1525
 100 °C
@Load 5.10 kg
212 °F
@Load 11.2 lb
ISO 306
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDENJ825 / 250169

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.