MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Aromatic

Material Notes: Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications include 3-dimensional parts such as V-rings, angle rings and spools, as well as barrier, gap spacers and core tubes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.730 g/ccCalculated number using basis weight and thickness
Thickness 1500 micronsASTM D374, method D, using 17 N/cm²
Linear Mold Shrinkage 0.0070 cm/cmASTM D3392
 0.015 cm/cmASTM D3392
Linear Mold Shrinkage, Transverse 0.010 cm/cmASTM D3392
 0.016 cm/cmASTM D3392
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 40.0 MPaASTM D828
Film Tensile Strength at Yield, TD 33.1 MPaASTM D828
Film Elongation at Yield, MD 11.2 %ASTM D828
Film Elongation at Yield, TD 12.9 %ASTM D828
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cm
@Temperature 130 °C
in oil; ASTM D257
 1.00e+18 ohm-cm
@Temperature 90.0 °C
in oil; ASTM D257
Dielectric Constant 3.2
@Frequency 60 Hz,
Temperature 25.0 °C
in oil; ASTM D150
 3.2
@Frequency 60 Hz,
Temperature 90.0 °C
in oil; ASTM D150
 3.3
@Frequency 60 Hz,
Temperature 130 °C
in oil; ASTM D150
Dielectric Strength 22.0 kV/mmAC rapid rise in air; ASTM D149
 34.0 kV/mmAC rapid rise in oil; ASTM D149
 73.0 kV/mmFull wave impulse in oil; ASTM D3426
Dissipation Factor 0.0050
@Frequency 60 Hz,
Temperature 25.0 °C
in oil; ASTM D150
 0.0050
@Frequency 60 Hz,
Temperature 90.0 °C
in oil; ASTM D150
 0.0070
@Frequency 60 Hz,
Temperature 130 °C
in oil; ASTM D150
 
Descriptive Properties
Basis Weight (g/m²)ASTM D3392

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® NN-33GF/000 L Nylon 66 - 33% Glass Fiber Reinforced - Internally Lubricated
Avient Edgetek® NN-33GF/000 HS Nylon 66 - 33% Glass Fiber Heat Stabilized
US Plastic Lumber Carefee Xteriors HDPE G/G Semi-Reinforced Plastic Lumber
Oxford Polymers Oxnilon 66-33GF 33% Glass Fiber Filled Nylon 66 for Injection Molding
Geon® Performance Solutions Vinyl Cellular E2010 Polyvinyl Chloride, Rigid

PMUE008 / 108389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.