MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Atom Adhesives AA-DUCT CG2 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulation. This concept opens the door to a wide range of applications previously prohibited by the much higher cost of Conventional silver conductive. AA-DUCT CG2 Formulated with Silver coated ceramic power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive substrates. AA-DUCT CG2 formulation produces electrically conductive paths on a wide variety of surfaces including plastics, rubber, cloth, thermoplastic, paper, wood and many others. AA-DUCT CG2 designed for use in diversified applications as microwave EMI & RFI shielding, in the assembly or repair of printed circuit boards, waveguides, electronic modules, flat cable, static shielding, connections, and circuitry.

Appearance: Silver Coated ceramic

Cure Type: Heat cure

Benefits:

  • High strength
  • Perfect bond
  • EMI & RFI shielding
  • Wave guides
Substrates: Excellent choice for the Integrated Circuits, aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.

Catalyst: Anhydride

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 6800 cP6800 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 4.14 GPa600 ksi
Poissons Ratio 0.350.35
Shear Strength 13.8 MPa2000 psicured
Adhesive Bond Strength 10.3 MPa1500 psicured
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.10 ohm<= 0.10 ohmcured
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.0 µm/m-°C31.7 µin/in-°Fcured
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°Fcured
Thermal Conductivity 4.18 W/m-K29.0 BTU-in/hr-ft²-°Fcured
 
Processing PropertiesMetricEnglishComments
Cure Time  42.0 min
@Temperature 200 °C
0.700 hour
@Temperature 392 °F
 90.0 min
@Temperature 180 °C
1.50 hour
@Temperature 356 °F
 150 min
@Temperature 160 °C
2.50 hour
@Temperature 320 °F
Pot Life 259200 min259200 minuncured
Shelf Life 6.00 Month6.00 Monthuncured
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 65 - 75 %65 - 75 %ceramic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® T905BN-3 Thermally Conductive Epoxy
Dow TC-5688 Thermally Conductive Compound
Dow TC-5022 Thermally Conductive Compound
Cotronics Resbond™ 920 High Temperature Ceramic Adhesive, Thermally Conductive
Cotronics 454B Machinable Non-Sag Putty Adhesive

PATOM049 / 172364

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.