System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
AISI 8645 Steel
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 8000 Series Steel
;
Low Alloy Steel
;
Carbon Steel
;
Medium Carbon Steel
Key Words:
SAE J404, SAE J412, SAE J770, UNS G86450, ASTM A322, ASTM A331, ASTM A505, ASTM A519, MIL-SPEC MIL-S-16974
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.85
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Brinell
184 - 235
Hardness, Knoop
239
Converted from Brinell
Hardness, Vickers
220
Converted from Brinell
Bulk Modulus
160
GPa
Typical for steel.
Shear Modulus
80.0
GPa
Typical for steel.
Component Elements Properties
Original Value
Comments
Carbon, C
0.43 - 0.48 %
Chromium, Cr
0.40 - 0.60 %
Iron, Fe
96.595 - 97.72 %
As remainder
Manganese, Mn
0.75 - 1.0 %
Molybdenum, Mo
0.15 - 0.25 %
Nickel, Ni
0.40 - 0.70 %
Phosphorus, P
<= 0.035 %
Silicon, Si
0.15 - 0.30 %
Sulfur, S
<= 0.040 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI 8720 Steel
AISI 8655 Steel
ASTM A283 Steel, grade A
AISI 8655H Steel
AISI 4130 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
M864EA / 8506
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.