MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch™ 2210 Vinyl Mastic Pads and Rolls
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are designed to insulate, moisture seal and pad all connections up to 600 volts, and have excellent resistance to abrasion, moisture, alkalies, acid, copper corrosion and varying weather conditions (including sunlight).

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.75 %0.75 %ASTM D570
Water Vapor Transmission 3.88 g/m²/day0.250 g/100 in²/dayASTM D3833
Thickness 178 microns7.00 milBacking; ASTM D1000
 2110 microns83.0 milMastic-Roll; ASTM D1000
 2290 microns90.0 milComposite-Roll; ASTM D1000
 3000 microns118 milMastic-Pad; ASTM D1000
 3180 microns125 milComposite-Pad; ASTM D1000
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 200 %200 %ASTM D1000
Peel Strength 2.19 kN/m12.5 pliAdhesion to Steel; ASTM D1000
 2.19 kN/m12.5 pliAdhesion to Polyethylene; ASTM D1000
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D1000
Dielectric Strength 11.8 kV/mm300 kV/inASTM D1000
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35181 / 169928

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.