MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical DOA Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Features: LG DOA is an aliphatic plasticizer and used to keep softness of product under cold water.

Application: Wrap for food package, synthetic leather, sheet, hose, gasket

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 11 cP
Molecular Weight 317 g/mol
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.10
@Treatment Temp. 125 °C,
Time 10800 sec
After Heating, KOH mg/g; JIS K6751
 
Thermal PropertiesOriginal ValueComments
Melting Point -70.0 °CFreezing Point
Boiling Point 335 °C
Flash Point 196 °C
 
Descriptive Properties
Acidity<0.03 KOH mg/gJIS K6751
Color<15 APHAJIS K6751
Ester Value299-305JIS K6751
Heat Loss<0.1%125°Cx3hr, JIS K6751

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical DINP Plasticizer
LG Chemical EM505 Impact modifier for Engineering Plastics
LG Chemical EM500A Impact modifier for Engineering Plastics
LG Chemical EM500 Impact modifier for Engineering Plastics
LG Chemical DOP Plasticizer

PLAY247 / 148257

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.