MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Lubrizol LifeSciences Isoplast® 2560 ETPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Isoplast® 2560 Natural is an engineering thermoplastic polyurethane resin for medical applications

Features: USP Class VI

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.71 g/cc1.71 g/ccASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 227 MPa32900 psiASTM D638
Tensile Strength, Yield 227 MPa32900 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Elongation at Yield 2.0 %2.0 %ASTM D638
Tensile Modulus 17.0 GPa2470 ksiASTM D638
Flexural Strength 393 MPa57000 psiASTM D790
Flexural Modulus 15.0 GPa2180 ksiASTM D790
Izod Impact, Notched  8.54 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
16.0 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 8.54 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
16.0 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
Dart Drop, Total Energy  25.0 J
@Temperature -29.0 °C
18.4 ft-lb
@Temperature -20.2 °F
ASTM D3763
 29.0 J
@Temperature 23.0 °C
21.4 ft-lb
@Temperature 73.4 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C6.11 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °Fannealed; ASTM D648
 127 °C261 °Funannealed; ASTM D648
Vicat Softening Point 186 °C367 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Isoplast® 2530 White ETPU
Lubrizol LifeSciences Isoplast® 2530 ETPU
Lubrizol LifeSciences Carbothane® AC-4055D-B20 Aromatic TPU
Lubrizol LifeSciences Isoplast® 2510 ETPU
Lubrizol LifeSciences Isoplast® 2531 ETPU

PLUBR9024 / 203591

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.