MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ LUBRICOMP™ Compound DX09407H Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DX09407H compound is based on High Heat Polycarbonate (PC) resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare.

Features: Healthcare,Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.210 %0.210 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psi5 mm/min; ASTM D638
 56.0 MPa8120 psi5 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa9280 psi5 mm/min; ASTM D638
 64.0 MPa9280 psi5 mm/min; ISO 527
Elongation at Break 68 %68 %5 mm/min; ASTM D638
 111 %111 %5 mm/min; ISO 527
Elongation at Yield 6.8 %6.8 %5 mm/min; ASTM D638
 6.9 %6.9 %5 mm/min; ISO 527
Tensile Modulus 2.13 GPa309 ksi1 mm/min; ISO 527
 2.23 GPa323 ksi5 mm/min; ASTM D638
Flexural Strength 90.0 MPa13100 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.08 GPa302 ksi2 mm/min; ISO 178
 2.30 GPa334 ksi1.3 mm/min, 50 mm span; ASTM D790
Flexural Strain at Break 76.8 %76.8 %2 mm/min; ISO 178
Izod Impact Notched 139 J103 ft-lbASTM D256
Izod Impact, Unnotched 22.14 J/cm41.48 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 191 kJ/m²90.9 ft-lb/in²80*10*4; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 139 °C
@Thickness 3.20 mm
282 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80759 / 288706

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.