MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SCIGRIP SG218 A Methacrylate Adhesive + SG218 B Activator
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: SCIGRIP® SG200 Series Methacrylate Adhesives are two-component, 10:1 mix ratio products for bonding composites, thermoplastics, metals and combinations thereof. Minimal surface preparation provides reduced labor and production cycle time. Widely used for marine, transportation and general plastic bonding applications.

Features: Minimal surface preparation, Non-sag handling characteristics, Excellent environmental resistance, Excellent fatigue, impact and shock load resistance.

Information provided by SCIGRIP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccAdhesive
 0.970 g/ccMix
 1.18 g/ccActivator
Viscosity 70000 - 180000 cPActivator
 170000 - 220000 cPAdhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2.50 - 3.00 ksi
Elongation at Break 60 - 100 %
Tensile Modulus 60.0 - 75.0 ksi
Adhesive Bond Strength 2200 - 2500 psiLap Shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 80.0 - 90.0 min
@Temperature 23.9 °C
Fixture Time
Working Life 35.0 - 45.0 min
@Temperature 23.9 °C
 
Descriptive Properties
ColorOff WhiteAdhesive
 WhiteActivator
 WhiteMix
Mix Ratio10:1 A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCIGR955 / 243179

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.