Applications: Rovene® 6025 can be used in multiple coating and paint applications including landscaping coatings and low sheen interior flat wall coatings. It can also be used as a binder for dust suppression and soil stabilization. Rovene® 6025 can be spray applied and coated by traditional methods. Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6025 Material Safety Data Sheet before handling, storing, or using this product. Information provided by Mallard Creek Polymers |