MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ FARADEX™ Compound ES003E Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP FARADEX ES003E compound is based on Polyetherimide (PEI) resin containing 15% stainless steel fiber. Added features of this grade include: Electrically Conductive, EMI/RFI shielding, Easy Molding.

Features: EMI/RFI Shielding,Electrically Conductive,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D792
Density 1.46 g/cc0.0527 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.190 %0.190 %23°C/50% RH/24 hrs; ASTM D570
 0.270 %0.270 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 98.0 MPa14200 psi5 mm/min; ISO 527
 105 MPa15200 psi5 mm/min; ASTM D638
Tensile Strength, Yield 99.0 MPa14400 psi5 mm/min; ISO 527
 105 MPa15200 psi5 mm/min; ASTM D638
Elongation at Break 4.3 %4.3 %5 mm/min; ISO 527
 5.0 %5.0 %5 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %5 mm/min; ISO 527
 4.8 %4.8 %5 mm/min; ASTM D638
Tensile Modulus 4.34 GPa629 ksi1 mm/min; ISO 527
 4.66 GPa676 ksi5 mm/min; ASTM D638
Flexural Strength 155 MPa22500 psi2 mm/min; ISO 178
Flexural Modulus 4.31 GPa625 ksi2 mm/min; ISO 178
 4.59 GPa666 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 34.0 J25.1 ft-lbASTM D256
Izod Impact, Unnotched 4.85 J/cm9.09 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 33.0 kJ/m²15.7 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 7.00 J5.16 ft-lbASTM D3763
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 89 ohm-cm89 ohm-cmASTM D257
Surface Resistance 10 - 1000 ohm10 - 1000 ohmASTM D257
Shielding Effectiveness 60 dB
@Thickness 2.50 mm
60 dB
@Thickness 0.0984 in
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 44.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
24.4 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 194 °C381 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 190 °C
@Thickness 3.20 mm
374 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 177 °C351 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 180 °C
@Thickness 3.20 mm
356 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 390 - 400 °C734 - 752 °F
Zone 2 370 - 390 °C698 - 734 °F
Zone 3 380 - 400 °C716 - 752 °F
Melt Temperature 360 - 400 °C680 - 752 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80630 / 288577

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.