MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8253 HS PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased flexibility. It is also available in non-heat stabilized (Ultramid 8253) and/or pigmented versions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 1.5 %24 hour; ISO Test
Linear Mold Shrinkage 0.012 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ASTM Test
Tensile Strength at Break 60.0 MPa0.2 in/min; ASTM Test
 100 MPa
@Temperature -40.0 °C
ASTM Test
 100 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Yield 65.0 MPa2 in/min; ASTM Test
 20.0 MPa
@Temperature 120 °C
ASTM Test
 20.0 MPa
@Temperature 120 °C
ISO Data
 25.0 MPa
@Temperature 80.0 °C
ISO Data
 25.0 MPa
@Temperature 80.0 °C
ASTM Test
 117 MPa
@Temperature -40.0 °C
ASTM Test
 117 MPa
@Temperature -40.0 °C
ISO Data
Elongation at Break >= 100 %2 in/min; ASTM Test
 9.0 %
@Temperature -40.0 °C
ASTM Test
 9.0 %
@Temperature -40.0 °C
ISO Data
Elongation at Yield 4.0 %2 in/min; ASTM Test
 7.0 %
@Temperature -40.0 °C
ASTM Test
 7.0 %
@Temperature -40.0 °C
ISO Data
 29 %
@Temperature 80.0 °C
ISO Data
 29 %
@Temperature 80.0 °C
ASTM Test
 34 %
@Temperature 120 °C
ASTM Test
 34 %
@Temperature 120 °C
ISO Data
Tensile Modulus 295 MPa
@Temperature 120 °C
ISO Data
 400 MPa
@Temperature 80.0 °C
ISO Data
 2835 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 65.0 MPaISO Data
 87.0 MPaASTM Test
 14.0 MPa
@Temperature 120 °C
ASTM Test
 20.0 MPa
@Temperature 93.0 °C
ASTM Test
 25.0 MPa
@Temperature 65.0 °C
ASTM Test
 148 MPa
@Temperature -40.0 °C
ASTM Test
Flexural Modulus 1900 MPaISO Data
 2210 MPaASTM Test
 260 MPa
@Temperature 120 °C
ASTM Test
 325 MPa
@Temperature 93.0 °C
ASTM Test
 415 MPa
@Temperature 65.0 °C
ASTM Test
Izod Impact, Notched 0.800 J/cm
@Temperature -40.0 °C
ASTM Test
 1.48 J/cm
@Thickness 3.17 mm
ASTM Test
 
Thermal PropertiesOriginal ValueComments
CTE, linear 99.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
Melting Point 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 168 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8350 HS PA6 (Dry)
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6
BASF Ultramid® 8253 HS BK-102 PA6 (Dry)
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
BASF Ultramid® 8260 HS PA6 (Dry)

PBASF9173 / 84937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.