MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C17530, TH04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard and Precipitation Heat Treated

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Spot Weld, Capacity for Being Hot Formed; Fair Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding, Seam Weld, Butt Weld

Typical Uses: Connectors terminals, miniature; Fuse Clips; IC Lead Frames; Relays; Springs; Switches; Bellows; Diaphragms

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 758 MPa110000 psi0.2% Offset
Elongation at Break >= 8.0 %>= 8.0 %
Tensile Modulus 128 GPa18500 ksi
Modulus of Rigidity 49.0 GPa7100 ksi
Poissons Ratio 0.300.30Calculated
Machinability 40 %40 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000450 ohm-cm0.00000450 ohm-cm38% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.418 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K90.0 BTU-in/hr-ft²-°F
Melting Point 1050 - 1081 °C1922 - 1978 °F
Solidus 1050 °C1922 °F
Liquidus 1081 °C1978 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 843 - 927 °C
@Time 60.0 sec
1550 - 1700 °F
@Time 0.0167 hour
Water
Hot-Working Temperature 649 - 954 °C1200 - 1750 °F
Precipitation Temperature >= 454 °C>= 850 °FAir
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.60 %<= 0.60 %
Beryllium, Be 0.20 - 0.40 %0.20 - 0.40 %
Copper, Cu 96.1 - 98 %96.1 - 98 %As Balance
Iron, Fe <= 0.20 %<= 0.20 %
Nickel, Ni 1.8 - 2.5 %1.8 - 2.5 %
Silicon, Si <= 0.20 %<= 0.20 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC17530x1 / 291605

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.