MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Poly Alloy PoLinker™ PL1010 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PoLinker PL1010 resin is a grafted coupling agent based on polypropylene which combines functional groups by using reactive extrusion. PL1010 resin can improve the polarity of the plastic to increase the compatibility between different materials.

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.902 g/cc0.902 g/ccASTM D792
Melt Flow 80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature <= 45.0 °C<= 113 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9797ASTM D2240
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 95.0 °C203 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 300 °C<= 572 °F
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Heat resistance310°C2% weight reduction
MAH Graft levelLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPALLOY000 / 278279

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.