MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hostaform® LX90Z XAP² ™ POM, UV Resistant
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Preliminary Data Sheet

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO 1183
Water Absorption at Saturation 0.75 %0.75 %ISO 62
Linear Mold Shrinkage, Flow 0.023 cm/cm0.023 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psi50mm/min; ISO 527-2/1A
Elongation at Yield 8.0 %8.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.70 GPa392 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 2.90 GPa421 ksiISO 178
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
Melting Point 166 °C331 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 147 °C297 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 125 °C212 - 257 °Fcavity
 180 - 200 °C356 - 392 °Fhot runner
Zone 1 170 - 175 °C338 - 347 °F
Zone 2 170 - 180 °C338 - 356 °F
Zone 3 175 - 185 °C347 - 365 °F
Zone 4 180 - 190 °C356 - 374 °F
Die Temperature 185 - 195 °C365 - 383 °F
Melt Temperature 180 - 195 °C356 - 383 °F
Drying Temperature 105 - 110 °C221 - 230 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 4.00 MPa<= 580 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo PULSE™ GX50 PC/ABS Engineering Resin
Trinseo PULSE™ A35-110 PC/ABS
Trinseo PULSE™ A35-105 PC/ABS
Celanese N-325 Nylon 6/6
Celanese N-276 Glass/Mineral Reinforced Nylon 6/6

PHCQ391 / 178846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.