MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos FM 1224 Non flame-retardant bedding compound for XLPE insulation and HFFR sheathing.
Categories: Polymer; Thermoplastic

Material Notes: Non flame-retardant bedding compound for XLPE insulation and HFFR sheathing.

Compound class: Bedding compound

Based on: IIR

Characteristics: Halogen free

Application examples: Insulation
2 XI 1; XLPE; acc. DIN / VDE 0207 part 22
2 YI 1 – 5; PE; acc. DIN / VDE 0207 part 2
9 YI 1; PP; acc. DIN / VDE 0207 part 7
3 GI 3; EPR; acc. DIN/VDE 0207 part 20

Application examples: Sheathing
HM 4 – 2; HFFR; acc. DIN / VDE 0207 part 24
2 YM 3; HDPE; acc. DIN / VDE 0207 part 3

Typical applications: Bedding compound for cables and wire with max. 90°C operating temperature at conductor

Features: For 2-step process (coilable); Halogen-free

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.84 g/cc0.0665 lb/in³pressed plaques, 100°C / 5 min.; DIN EN ISO 1183-1A
Mooney Viscosity 45
@Temperature 100 °C
45
@Temperature 212 °F
ML (1+4); DIN ISO 289-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050pressed plaques, 100°C / 5 min.; DIN ISO 7619-1
Tensile Strength >= 1.00 MPa>= 145 psipressed plaques, 100°C / 5 min.; IEC 60811-501
Elongation at Break >= 250 %>= 250 %pressed plaques, 100°C / 5 min.; IEC 60811-501
 >= 150 %
@Temperature 120 °C,
Time 605000 sec
>= 150 %
@Temperature 248 °F,
Time 168 hour
pressed plaques, after ageing; DIN EN 60811-401
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm
@Temperature 27.0 °C
>= 1.00e+12 ohm-cm
@Temperature 80.6 °F
VDE 0472 Part 503
Surface Resistance >= 1.00e+9 ohm
@Temperature 23.0 °C
>= 1.00e+9 ohm
@Temperature 73.4 °F
VDE 0472 Part 502
 
Processing PropertiesMetricEnglishComments
Processing Temperature 95.0 - 105 °C203 - 221 °FTool
 95.0 - 105 °C203 - 221 °FMaximum mass temperature
Zone 1 70.0 - 80.0 °C158 - 176 °F
Zone 2 75.0 - 85.0 °C167 - 185 °F
Zone 3 85.0 - 95.0 °C185 - 203 °F
Zone 4 85.0 - 95.0 °C185 - 203 °F
Adapter Temperature 90.0 - 110 °C194 - 230 °F
Head Temperature 95.0 - 105 °C203 - 221 °F
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 22 %22 %pressed plaques, 100°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Screw60-70°C
Wallace-Plasticity= 50%BS 903

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS063 / 296170

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.