MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® N-276 NF3001 40% Glass/Mineral Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: Ultramid N-276 NF3001 is a 40% mineral/glass reinforced, heat stabilized injection molding nylon 6/6.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 135 MPa5mm/min; ISO 527
Elongation at Break 3.0 %5mm/min; ISO 527
Tensile Modulus 10800 MPa1mm/min; ISO 527
Flexural Modulus 6900 MPaASTM Test
 9800 MPaISO Data
Izod Impact, Notched (ISO) 4.20 kJ/m²ISO Test
Charpy Impact Unnotched 4.50 J/cm²ISO 179
 4.00 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.380 J/cm²ISO 179
 0.350 J/cm²
@Temperature -30.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 257 °C10 K/min
 257 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 255 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 241 °CASTM Test
 242 °CISO 75
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Basantol® X82 Black Liquid
BASF Basantol® 311 Red Liquid
BASF Basantol® 273 Orange Liquid
BASF Basantol® 215 Yellow Liquid
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE

PBASF9379 / 85143

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.