MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2899 X 106530 A Value-added Thermoplastic Polyolefin Elastomer, Nylon 6 Overmolding
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D 792
Linear Mold Shrinkage 0.013 - 0.017 cm/cm
@Thickness 3.17 mm
0.013 - 0.017 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 454510 s delay; ASTM D 2240
Tensile Strength at Break 2.76 MPa
@Thickness 3.17 mm
400 psi
@Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Tensile Stress at Strain  1.03 MPa
@Strain 50 %,
Thickness 3.17 mm
150 psi
@Strain 50 %,
Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
 1.38 MPa
@Strain 100 %,
Thickness 3.17 mm
200 psi
@Strain 100 %,
Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
 2.55 MPa
@Strain 100 %,
Thickness 3.17 mm
370 psi
@Strain 100 %,
Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Elongation at Break 360 %
@Thickness 3.17 mm
360 %
@Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Tear Strength 14.0 kN/m80.0 pliDie C; ASTM D 624
Peel Strength 3.16 kN/m18.0 pliNylon 6; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set  17 %
@Temperature 23.0 °C,
Time 79200 sec
17 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 39 %
@Temperature 70.0 °C,
Time 79200 sec
39 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 282 °C480 - 540 °F
Mold Temperature 37.8 - 71.1 °C100 - 160 °F
Drying Temperature 79.4 °C175 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.080 %<= 0.080 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 34.5 - 103 MPa5000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
Overview of materials for Silicone Polyurethane, Polycarbonate Based

PQZWA2753 / 91356

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.