MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultramid® PSB 286 NATURAL Nylon 6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Product Description: Ultramid® PSB 286 is an unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding. This grade offers high fluidity and good mold release.

Availability: North America

Uses: Consumer Applications; Industrial Applications

Agency Ratings: EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Natural Color; Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Maximum Moisture Content 0.20
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5950 psiISO 527-2
Tensile Strength, Yield 6530 psiISO 527-2
Tensile Modulus 189000 psiISO 527-1
Flexural Strength 5800 psiISO 178
Flexural Modulus 145000 psiISO 178
Charpy Impact, Notched 39.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+12 ohmIEC 62631-3-2
Dielectric Constant 3.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 460 V/mil
@Thickness 2.00 mm
IEC 60243-1
Dissipation Factor 0.10
@Frequency 100 Hz
IEC 62631-2-1
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 446 - 455 °F
Middle Barrel Temperature 455 - 464 °F
Front Barrel Temperature 455 - 473 °F
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2055 / 310748

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.