MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sirmax Dafneohm® 6A KP06 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Reinforced polyamide 6. Good impact resistance and good processability. Partially conductive/dissipative.

Application: Injection Molding

Information provided by Sirmax®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 - 1.34 g/cc0.0477 - 0.0484 lb/in³ISO 1183
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psi5 mm/min; ISO 527-2
Elongation at Break 5.0 %5.0 %5 mm/min; ISO 527-2
Tensile Modulus 14.0 GPa2030 ksi1 mm/min; ISO 527-2
Flexural Strength 220 MPa31900 psi2 mm/min; ISO 178
Flexural Modulus 14.0 GPa2030 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5000 ohm-cm5000 ohm-cmIEC 60093
Surface Resistance 5000 ohm5000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 165 °C329 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75/Af
Vicat Softening Point 210 °C410 °FB50; ISO 306
 215 °C419 °FA50; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Ignition Temperature  675 °C
@Thickness 1.00 mm
1250 °F
@Thickness 0.0394 in
IEC 60695-2-13
 675 °C
@Thickness 2.00 mm
1250 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index  650 °C
@Thickness 1.00 mm
1200 °F
@Thickness 0.0394 in
IEC 60695-2-12
 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °FISO 294
Mold Temperature 60.0 - 80.0 °C140 - 176 °FISO 294
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIRMX036 / 281139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.