MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANADD® LASER AD Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® LASER AD is a very high reactive Laser additive Masterbatch added into TPU granules. We recommend the product in combination with our PEARLTHANE–TPU’ s: PEARLTHANE D11TXX – range; PEARLTHANE D15NXX – range; PEARLTHANE D16NXX – range With the adding of DANADD® LASER AD, together with the classical colorless TPU’ s, Laser signs are equipped properly. DANADD® LASER AD will delivered in standard form as yellow colored granules. Other color adjustments will be delivered on demand.

Application: DANADD® LASER AD is added during the injection molding process together with TPU’ s in a metering mixing unit. We recommend for the classical TPU – Laser signing a addition of 2%– 8% DANADD® LASER AD with Polyester- or Polyether- TPU’ s.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Softening Point 180 °CKOFLER
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 230 °CKOFLER
Shelf Life 6.00 Month
 
Descriptive Properties
Active content0.2Volume
Aspectyellow colored, even cylinder granules
Dosage2-8%
Heat resistance by the processing5 min235°C
Humidity< 0,05%Rest

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ005 / 294425

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.