Glass Fiber 20% - PTFE 10% - FDA Type Comments: - Glass Fiber
- PTFE Lubricated
- FDA Compliant
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |