MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemours Teflon™ PFA 9725 Molding and Extrusion Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Teflon™ PFA 9725 is a general-purpose fluoroplastic resin available as loosely compacted fluff. It is intended for use in special application processes in consultation with Chemours. Compared with other grades of Teflon™ PFA, its most unique features are a relatively low flow rate and properties that make it suitable for a variety of processes and demanding end uses, especially compounding and compression molding. Teflon™ PFA 9725 is an ideal resin for applications involving compounding and compression molding, as well as extruded tubing and other profiles for hose, electrical insulators, and sleeving; industrial film and products made from film; and injection or blow-molded articles requiring superior electrical, chemical, and thermal properties. Teflon™ PFA 9725 offers a slightly lower melt flow rate than Teflon™ PFA TE9724, ultimately providing a higher degree of stress-crack resistance.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
Melt Flow 1.7 g/10 minASTM D3307
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength 26.0 MPaASTM D3307
Elongation, Ultimate 300 %ASTM D3307
Flexural Modulus 0.625 GPaASTM D790
Flex Crack Resistance 500000
@Thickness 0.203 mm
Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohmASTM D257
Dielectric Constant 2.03
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.250 mm
Short Time; ASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 305 °CASTM D4591
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D240
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Heat of Combustion5.3 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceOutstanding
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8815 / 268741

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.