MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Adstif HA620J HP PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Adstif HA620J HP is a high stiffness polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It has a very low level of catalyst residues and it does not contain any slip and antiblocking agents. Adstif HA620J HP offers good optical, easy processing and good film profile.

Availability: Africa-Middle East; Europe

Application: Barrier Film; Food Packaging Film

Market: Flexible Packaging

Processing Method: BOPP

Attribute: Good Dimensional Stability; High Gloss; High Purity; High Stiffness; Homopolymer; Low Catalyst Residuals

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 3.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 21.0 MPa3050 psi50 mm/min; ISO 527-1, -2
Tensile Strength, Yield 37.0 MPa5370 psi50 mm/min; ISO 527-1, -2
Elongation at Break 100 %100 %50 mm/min; ISO 527-1, -2
Elongation at Yield 9.00 %9.00 %50 mm/min; ISO 527-1, -2
Flexural Modulus 1.75 GPa254 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 160 °C320 °FA/50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9013 / 323941

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.