MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aurora Plastics TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Application: High impact resistant, non-blooming flame retardant polypropylene compound designed for UL94 V-0 injection molding applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 - 1.02 g/ccASTM D792
Melt Flow 15 - 21 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 1500 psiASTM D2863
Tensile Strength, Yield >= 3700 psiASTM D638
Elongation at Break >= 50 %ASTM D638
Flexural Modulus 1380 MPaASTM D790
Izod Impact, Notched >= 1.20 ft-lb/inASTM D256
Dart Drop Total Energy >= 6.41 J/cmASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 186.7 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
Oxygen Index >= 28 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aurora Plastics TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant
Asahi Kasei Thermofil P-20TC-Y178 20% Talc Reinforced, Flame Retardant, Heat Stabilized Polypropylene
Celanese SO.F.TER Polifor® QD 813 Y001 WOD Flame Retardant Polypropylene
Celanese SO.F.TER Polifor® QD 813 30% Glass Fiber Reinforced Self Extinguishing Polypropylene, Flame Resistant
Celanese SO.F.TER Polifor® 5220/V0-EP Mineral Filled Self Extinguishing Polypropylene, Flame Resistant

PSEPN121 / 179125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.