MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Rubaloy Rubaloy L 7360 NBR / PVC
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Information: Rubaloy L 7360 is a non-staining, oil, ozone, abrasion, weather and flex resistant polymer using low (28%) Acrylonitrile Butadiene Rubber and a special grade of Poly Vinyl Chloride Resin Blend which can easily withstand low temperatures of upto -45°C. This grade offers excellent rubber- to- metal bonding.

Processing Characteristics: Easily processable on conventional Rubber processing / compounding Machines. Very good filler and plasticizer absorption makes compounding cycle quick, cost saving and labour saving. Warm mixing mill compounding is recommended for best results. It can easily withstand elevated compounding temperatures. Recommended plasticizers are DOA, DOS, TCR, and other Aromatic Plasticizers. Paraffinic based softeners are not recommended.

Applications: Low Temperature flex resistant products, Gasoline Tubings and Hose Covers, Conveyor Belt covers, LPG Tubing, Auto Parts, Gaskets, Oil Seals, Oil Resistant and antistatic Shoe Soles, Rubber Sheets and Extruded Rubber Parts, Textile Cots, Aprons, Industrial Textile and Printing Rolls, Expanded Sheets for insulation, Auto weather strips etc.

Advantages over regular NBR/PVC 70:30 Blends :

  • Excellent low temperature flex properties upto - 45°C.
  • Excellent processability.
  • Improved compression set.
  • Controlled swelling.
  • Excellent rubber-metal bonding.

Information provided by Rubaloy™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 - 1.06 g/cc
Mooney Viscosity 60 - 70
@Temperature 100 °C
ML 1+4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55 - 65
 
Descriptive Properties
ACN Content0.28
Extraction Percentage>1%
Polymer Ratio70:30
StabilizerNon-Staining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRUBAL004 / 317268

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.